Preparation and Characterization of Paclitaxel Loaded Polymer Vesicle Formulations
Shuliang Li1, Belinda M. Byrne2, JoEllen J. Welsh3 and Andre F. Palmer1, (1)Department of Chemical and Biomolecular Engineering, University of Notre Dame, 181 Fitzpatrick Hall,, Notre Dame, IN 46556, (2)Department of Biological science, University of Notre Dame, Notre Dame, IN 46556, (3)Department of Biological Science, University of Notre Dame, Notre Dame, IN 46556

Vesicles self-assembled from polyethylene oxide-b-polylactide(PEO-PLA), polyethylene oxide-b-polycaprolactone (PEO-PCL) and polyethylene oxide-b-polybutadiene (PEO-PBD) diblock copolymers were encapsulated with paclitaxel. The morphology of self-assembled PEO-PBD colloids was studied using atomic force microscopy (AFM). It was observed that the structure of these polymer colloids ranged from spherical micelles, worm-like micelles, to polymersomes depending on the diblock composition and preparation method. The in vitro release of paclitaxel in PBS buffer, size distribution, and in vitro stability of paclitaxel loaded polymer vesicles was studied. The loading content of paclitaxel in polymer vesicles was in the range of 4.1-13.5 wt.% depending on the block composition of diblock copolymers, the weight ratio of paclitaxel to block copolymer, and the morphology of the self-assembled diblock copolymer colloids. The in vitro cytotoxicity evaluation of paclitaxel loaded polymer vesicles on MCF7 human breast cancer cells shows that the paclitaxel loaded polymer vesicles exhibit comparable activity to that observed with free paclitaxel at 0.01 ėg/mL of paclitaxel.

Extended Abstract Status: Not Uploaded

Poster Session: Drug and Gene Delivery

The Preliminary Program for 2005 Annual Meeting (Cincinnati, OH)