Preliminary Program subject to change
Session 13: Future Directions
Presentation TypeOral
Summary Statement
Superelastic NiTi Interlayers for Improving the Wear Resistance of Hard Coatings on Soft Substrates
Mr. Yijun Zhang1, Dr. David S. Grummon1, Dr. Yang-Tse Cheng2 and Dr. John A. Shaw3, 1Chemical Engineering and Materials Science, Michigan State University, 3525 Engineering Blg., East Lansing, MI 48824-1226, 2Research and Development, General Motors, Materials and Processes Laboratory, Warren, MI 48090, 3Department of Aerospace Engineering, The University of Michigan, 1320 Beal Ave, FXB Bldg., Ann Arbor, MI 48109
Structure, Phase Transformation and Mechanical Property in Nanostructured TiNi Obtained by Severe Plastic Deformation
Prof. Koichi Tsuchiya1, Akihide Hosokawa1, Masayuki Katahira1, Yoshikazu Todaka1, Minoru Umemoto1 and Dr. Koichi Morii2, 1Production Systems Engineering, Toyohashi University of Technology, Tempaku-cho Hibarigaoka 1-1, Toyohashi, 441-8580, Japan, 2Research and Development Laboratory, Daico Steels, Co., Ltd., Daido-cho 2-30, Higashi-ku, Nagoya, 457-8545, Japan
Carbon and Oxygen Levels in Nitinol Alloys and the Implications for Medical Device Manufacture and Durability
Dr. Neil B. Morgan, John DiCello, Matt McGrane and Christine Trepanier, Nitinol Devices and Components, 47533 Westinghouse Drive, Fremont, CA 94539
Panel Discussion
Refreshment Break and Poster Viewing for Session 13 and 14

Online Submissions